Laserfiche WebLink
<br />SUBARTICLE 400-21.3 (page 407) is deleted and the following substituted: <br /> <br />400-21.3 Classification of Cracks: The Engineer will classify cracks as either <br />nonstructural or structural and determine the cause. In general, nonstructural cracks are cracks <br />1/2 inch or less deep from the surface of the concrete; however, the Engineer may determine that <br />a crack greater than 1/2 inch deep is nonstructural. In general, structural cracks are cracks that <br />extend deeper than 1/2 inch. A crack that is fully or partially underwater at any time during its <br />service life will be classified as a structural crack unless the Environment note on the General <br />Notes sheet in the plans categorizes the substructure as slightly aggressive, in which case, the <br />non structural crack criteria may apply as determined by the Engineer. <br />Review and comment on the Engineer's crack classification; however, the <br />Engineer will make the final determination. <br />